NAC standard
Dear friends! I have a question regarding the NAC transmission diffraction standard, which is Na2Ca3Al2F14. Is this standard safe in use, i.e., do I need any special safety when grinding it? Best regards! -- Łukasz Kruszewski, Ph.D., adjunct Polish Academy of Sciences Institute of Geological Sciences X-Ray Diffraction Laboratory (coordinator) Twarda 51/55 str. 00-818 Warsaw Poland ++ Please do NOT attach files to the whole list alan.he...@neutronoptics.com Send commands to lists...@ill.fr eg: HELP as the subject with no body text The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/ ++
Re: NAC standard
...don't breathe it in, don't eat, nor drink, and wear safety glasses,... Lovely :) Zitat von Andy FITCH fi...@esrf.fr: Dear ?ukasz, NAC is not a standard as it has never been subjected to any sort of formal procedure to ascertain its characteristics. Indeed each batch can be different. However, it is often highly crystalline, and so gives sharp peaks in a powder diffraction pattern, depending on which batch of sample it is. In terms of safety in handling it, I would suggest using normal safe powder-handling procedures; don't breathe it in, don't eat, nor drink, and wear safety glasses, lab coat, etc. . But why are you grinding it? Won't that affect the nice microstructure you're exploiting? And if it ever were certified as some sort of standard, grinding it is not the thing to do. Best regards Andy On 02/03/2014 16:10, ?ukasz Kruszewski wrote: Dear friends! I have a question regarding the NAC transmission diffraction standard, which is Na2Ca3Al2F14. Is this standard safe in use, i.e., do I need any special safety when grinding it? Best regards! ++ Please do NOT attach files to the whole list alan.he...@neutronoptics.com Send commands to lists...@ill.fr eg: HELP as the subject with no body text The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/ ++
Re: NAC standard
On 3 March 2014 12:30, Tomce Runcevski t.runcev...@fkf.mpg.de wrote: ...don't breathe it in, don't eat, nor drink, and wear safety glasses,... Lovely :) OK :-) AVOID breathing it in, don't eat, nor drink IN A LABORATORY, and wear safety glasses... It's not a joke. Those precautions should be second nature, especially in a chemistry or radiation laboratory. Alan __ * Dr Alan Hewat, NeutronOptics, Grenoble, FRANCE * alan.he...@neutronoptics.com +33.476.98.41.68 http://www.NeutronOptics.com/hewat __ ++ Please do NOT attach files to the whole list alan.he...@neutronoptics.com Send commands to lists...@ill.fr eg: HELP as the subject with no body text The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/ ++
Re: Na2Ca3Al2F14 (NAC) standard
be careful NAC is a great standard, but it is not certified, and different batches of the material have different broadening Nice to calibrate the angles, pay attention to calibrate the FWHM. Prof. Gilberto Artioli Dipartimento di Scienze della Terra Universita' degli Studi di Milano Sezione di Mineralogia Via Botticelli 23 I-20133 Milano tel: 39-02-5031 5609 fax: 39-02-5031 5597 personal e-mail: [EMAIL PROTECTED] secretary e-mail: [EMAIL PROTECTED] url: http://iummix.terra.unimi.it/~artioli/start.html -
Re: Na2Ca3Al2F14 (NAC) standard
Try the CNRS lab Laboratoire de Fluorures at the Université du Maine in 72000 Le Mans, France. Armel Le Bail will know, whom to ask ;-) Thomas On 05 Mar 2004, at 14:03, Magnus H. Sørby wrote: I want to purchase some standard Na2Ca3Al2F14 (NAC) powder to calibrate an Inel PSD. Does anybody know where I can get it? Magnus H. Sørby Ph.D. student Institute for Energy Technology University of Oslo Dep. of Physics Dep. of Chemistry Kjeller, Norway Oslo, Norway -- Dr. Thomas C Hansen, DS/DIF, ILL4-138 Institut Max von Laue-Paul Langevin, 6 rue Jules Horowitz, BP 156, F-38042 Grenoble Cedex 9 Phone +33 47620-7044, Fax +33 47620-7648 http://www.ill.fr/YellowBook/D20, mailto:[EMAIL PROTECTED]
Re: Na2Ca3Al2F14 (NAC) standard
You will need to contact: Prof. G. Courbion [EMAIL PROTECTED] Laboratoire des Fluorures UMR6010 Faculte de Sciences et Techniques Av O. Messiaen 72085 Le Mans cedex 9 A. Llobet Magnus H. Sørby wrote: I want to purchase some standard Na2Ca3Al2F14 (NAC) powder to calibrate an Inel PSD. Does anybody know where I can get it? Magnus H. Sørby Ph.D. student Institute for Energy Technology University of Oslo Dep. of Physics Dep. of Chemistry Kjeller, Norway Oslo, Norway -- === Dr. Anna Llobet Megias Lujan Neutron Scattering Center Los Alamos National Laboratory MSH805 Los Alamos, NM 87545 Phone: (505) 665-1367 Fax: (505) 665-2676 e-mail: [EMAIL PROTECTED] === License Exception: TSPA