Re: [RCSE] Post curing West System 105/206

2007-12-22 Thread Anker Berg-Sonne
Bill, I use Pro Set and it has all the post curing information right on it. Its a two phase curing process and I don't remember exactly what the times are, but I seem to remember 105 degrees for 24 hours. It does depend on the brand and model. As far as I remember, West Systems doesn't

[RCSE] Post curing West System 105/206

2007-12-21 Thread Bill Bunny Kuhlman
Granddaughter Alyssa and I are involved in vacuum bagging processes: carbon fiber spar caps, fiberglass over foam flying surfaces, and a molded all glass fuselage pod and boom. We're using West System 105/206 for all of the components. We know that post curing - higher than room temperature