Phen formula from ecatbuilder.com

The Ni powder, most pure and finest grade, is handled in dry box under
inert atmosphere. It is mixed with 5 % by weight carbon powder,
subjected to 500 C and degassed with a vacuum pump to prepare the
surface and clean out any oxygen/oxides clinging to it. The surface is
cooled. The chamber is pressurized with hydrogen to 2000 psi and
heated to 200 C after the gas line is closed. When the pressure
reaches stability the chamber is cooled. This process is repeated five
times to fully load the Ni. This reactive powder is mixed with 10% by
weight ferro magnetic Fe powder and an equal weight of magnesium
powder using the same careful techniques given above. 2 grams of this
mix is placed in an 8 inch lenth of 1/4  h Cu tube welded shut at one
end. The open end is fitted with a hydrogen uptake valve. A second 3/4
 gcopper tube is capped at one end and filled with mineral oil after
inserting the reaction chamber. The tube is placed in the center of a
1000   coil of magnetic copper wire such as Belden Part No. 8054 which
is connected to a source of alternating voltage adjustable from 25
cycles per second to 100 MHz. Using a thermocouple immersed in the
oil, connected to an old computer, the RFG is adjusted to supply
inductive energy to the Fe powder within the inner chamber raising the
temperature to 250 C. The fusion is adjusted to self sustain and
allowed to maintain the process for one year."