On 6/29/2006 1:09:01 AM, [EMAIL PROTECTED] wrote:
> Well, if the annealoing being discussed is the same as the technique 
> I use,
> then that woild be consistent.
>
> When working with PE (photo-etch) parts when building models, I 
> sometimes
> heat the part until it glows a bit, then allow it to cool slowly.
> Supposedly, this allows the part to be more easily bent, folded, 
> etc. The
> material
> I'm using is either brass or nickel. Never tried with copper though 
> (and stainless steel is right out and unbendable at this scale)...
>
 Yes, the Yield Strength of Stainless is far higher than brass of 
nickel.



xponent
Ductility Maru
rob 