Are you folks refering to the Willie Beutler's 2 part developer?  IF so,
here it is:

Part A

Water (distilled).......................500 ml
metol.......................................5 grams
Sodium Sulfite.........................25 grams

Part B

Water....................................500 ml
sodium carbonate....................25 grams

To use mix 1 part A with 1 part B + 100 parts water.  medium speed fils
hould develop between 8 and 12 minutes @ 65 degrees.
Do not use warmer temps.

Works great. I used this a long time ago. This is not a fine grain
developer, it is a sharpness developer. I stopped using this because Rodinal
gives just as good results without being as temperature fussy.

Joe Portale
Tucson, AZ

----- Original Message -----
From: <[EMAIL PROTECTED]>
To: <[EMAIL PROTECTED]>
Sent: Tuesday, July 31, 2001 9:59 AM
Subject: Re: [Cameramakers] What film type?


> > On Mon, 30 Jul 2001, peter davidoff wrote:
> > <http://rmp.opusis.com/formulae/formulae.html>.
>
> Don't have Beutler's formula either,  but a couple additional
> formulas (translated from German):
>
> http://www.larsmichael.com/reference/formulas.html
>
> Lars
> --
> Lars Michael                        [EMAIL PROTECTED]
> 87GT                             http://www.larsmichael.com/
> _______________________________________________
> Cameramakers mailing list
> [EMAIL PROTECTED]
> http://rmp.opusis.com/mailman/listinfo/cameramakers

_______________________________________________
Cameramakers mailing list
[EMAIL PROTECTED]
http://rmp.opusis.com/mailman/listinfo/cameramakers

Reply via email to