Cast acrylic from Laird Plastics in RI.  Give them the old ones and they will 
replicate.
________________________________
From: CnC-List <cnc-list-boun...@cnc-list.com> on behalf of Morgan Ellis via 
CnC-List <cnc-list@cnc-list.com>
Sent: Tuesday, August 27, 2019 10:21:11 PM
To: cnc-list@cnc-list.com <cnc-list@cnc-list.com>
Cc: Morgan Ellis <mje.mjel...@gmail.com>
Subject: Re: Stus-List 33-2 portlight material

Hi Dave, I used 6mm acrylic with a light bronze tint when I did mine this 
spring and it matched the original perfectly. It is my understanding that the 
UV and scratch resistant polycarbonate get those added properties from coatings 
applied to the surface and that these coatings don't last that long. Also I 
believe that Lewmar used acrylic on their hatches but it is much thicker, 
somewhere around 12mm.

Morgan Ellis
30-2
_______________________________________________

Thanks everyone for supporting this list with your contributions.  Each and 
every one is greatly appreciated.  If you want to support the list - use PayPal 
to send contribution --   https://www.paypal.me/stumurray

Reply via email to