At 05:55 5/17/98 +0000, you wrote:
>

>My procedure has been to clamp the piece between the bending blocks on a
>vice.  Then smack at the aluminum with a ball pein hammer.  After
>looking at the piece it is now apparent that this is not correct....
>Kevin
>

You are just one step away from the bends you want.
To be gentle with this soft material, you need to pat it with a 
soft-face mallet.
There are several options:
on the traditional side, a wooden or leather face mallet
on the modern side, a platic face mallet (with those yellow
 plastic end buttons)
or a dead-blow plastic faced hammer.

Brian Whatcott   Altus OK

-----------------------------------------------------------------------------