On Wed, 31 Mar 2021 at 03:40, Gene Heskett <[email protected]> wrote:

> the global flow to 80%, it laid a brim so-so with the head gap reduced
> by .1mm, and I went back up to 80C/245C, but 4 layers up its still
> slobbering and laying extra plastic that looks like snow.

The bed temp and extrude temp seem high. I do PETG at 65 / 230 and PLA
at 65 / 190.

Is it possible that the filament is damp? Has it been left out in the
atmosphere for weeks?

-- 