Hi,

I got some 2mm spacers from eBay (cant find the auction now) and let
some 0.9mm thick insulators be made in China (not used yet)..

Dalibor

2014-02-13 12:50 GMT+01:00 John Rehwinkel <[email protected]>:
>> My experimental tube without mercury is at ~1500 hrs, no signs of
>> metal deposit on glass, some deposit of shiny metal on ceramic
>> insulators
>
> Where did you get the ceramic insulators?
>
> - John
>
> --
> You received this message because you are subscribed to the Google Groups 
> "neonixie-l" group.
> To unsubscribe from this group and stop receiving emails from it, send an 
> email to [email protected].
> To post to this group, send an email to [email protected].
> To view this discussion on the web, visit 
> https://groups.google.com/d/msgid/neonixie-l/A139F719-1079-439A-A21D-E77FB01CF0AE%40mac.com.
> For more options, visit https://groups.google.com/groups/opt_out.



-- 
Dalibor Farny
----------------------------------------
phone: +420 724 321 571
http://www.daliborfarny.com
blog: http://dalibor.farny.cz

-- 
You received this message because you are subscribed to the Google Groups 
"neonixie-l" group.
To unsubscribe from this group and stop receiving emails from it, send an email 
to [email protected].
To post to this group, send an email to [email protected].
To view this discussion on the web, visit 
https://groups.google.com/d/msgid/neonixie-l/CA%2BnkT5p3mo4oo_5H73wfyc1-YMzScLsaCK0neHV%2BHZ1xkXAQ-A%40mail.gmail.com.
For more options, visit https://groups.google.com/groups/opt_out.

Reply via email to