At 12:31 PM 4/26/99 -0400, you wrote:
>       Scanned data from a Guinier camera film in a tab delimited XY text file
>allows the graphic presentation of the data in a report.  I would like to
take
>it one step further and try to refine model sturctures for unkown phases in
>GSAS.  Does anyone have a program which will do this (LINUX or Windows-95).
>
>       Not being a programmer, I have tried some software off the web.  The
>program "Convert" will output an XY format from GSAS but does not seem to
>import XY into GSAS.  "Winfit" will open the XY file and allowed me to peak
>picks and convert the arbitrary X units into a two theta scale using silcon
>peaks present as an internal standard.  In principle "Winfit" should be
able to
>export into file formats which could be imported into GSAS.  In practice
there
>are problems with the headers or formatting which prevents this.
>
>Thankyou
>
>Roger M. Sullivan
>Deptartment of Chemistry
>North Carolina State University
>Raleigh NC
>[EMAIL PROTECTED]
>

Dear Sir,

PowderX program (under Win95/98) can read in X-Y (two column, Intensity
versus 2theta) data and output data format for many structure-solution and
rietveld program including GSAS. You should edit the XY files before you
use PowderX so that it have two header lines: 
First Line: Sample Name or any informations with size <= 80 characters. 
Second Line: Total number of the data point.
Third line to End: two column table of 2theta vs. Intensity data pairs.

Best wishes

Cheng Dong


Dr. Cheng Dong                 
Institute of Physics        | Tel. 86-10-62582173
Chinese Academy of Sciences | Fax. 86-10-62568834
P.O.Box 603, Beijing 100080,|E-mail [EMAIL PROTECTED] 
P.R. China                  |

Reply via email to