The latest 1998 J.I. Langford LAPOD Powder Unit Cell Refinement
Software in the form of Fortran source code, DOS executable and
example file is available at.
http://www.ccp14.ac.uk/ccp/web-mirrors/lapod-langford/
This also includes some comments by J.I.Langford on using
LAPOD and correctiing powder data for instrumental peak shifts.
------
If you compile up a version of this for other operating systems
for active use, please feel free to make this available on the web
or E-mail this in for adding on the LAPOD web-area.
Lachlan.
--
Lachlan M. D. Cranswick
Collaborative Computational Project No 14 (CCP14)
for Single Crystal and Powder Diffraction
Daresbury Laboratory, Warrington, WA4 4AD U.K
Tel: +44-1925-603703 Fax: +44-1925-603124
E-mail: [EMAIL PROTECTED] Ext: 3703 Room C14
NEW CCP14 Web Domain (Under heavy construction):
http://www.ccp14.ac.uk