Hi everybody ! I have had some problems to set the correct preferred orientation direction.I have tried to get the axis zone direction from the peaks that I suppose are raised and so supply this direction to Fullprof as pr1,pr2 and pr3, but this is not working well.Then, my question is : how can I get the preferred orientation direction (pr1,pr2,pr3)from an X-ray pattern expressed in reciprocal space? Thanks .
- Re: preferred orientation Jo�o Batista Santos Barbosa
- Re: preferred orientation Anonymous