>  Does anyone know of a shareware program that can convert files in the
> (Siemens) *.raw format to the (Philips) *.rd format? Thanks in advance,

Two options:

WinFIT by Stefan Krumm 
(is meant for Peak Profiling but can open and save as either:
   http://www.geol.uni-erlangen.de/html/software/winsoft.html
Mirrors:
   http://www.ccp14.ac.uk/ccp/web-mirrors/krumm/html/software/winsoft.html
   http://ccp14.sims.nrc.ca/ccp/web-mirrors/krumm/html/software/winsoft.html
  

ConvX - mass data converter for Windows by Mark Bowden.
   http://www.ceramics.irl.cri.nz/Convert.htm

Lachlan.

-- 
Lachlan M. D. Cranswick

Collaborative Computational Project No 14 (CCP14)
    for Single Crystal and Powder Diffraction
Daresbury Laboratory, Warrington, WA4 4AD U.K
Tel: +44-1925-603703  Fax: +44-1925-603124
E-mail: [EMAIL PROTECTED]  Ext: 3703  Room C14
                           http://www.ccp14.ac.uk