>Could anyone provide me refinement data of yttrium aluminium garnet (YAG)
>and Gadolinium gallium garnet (GGG) or tell me where to find it?
Do not forget that Nature already built many minerals.
There are several garnets at the American Mineralogist Crystal
Structure Database :
http://www.geo.arizona.edu/xtal-cgi/test
And when your Rietveld fit will be OK, send your raw powder
data to PowBase : http://sdpd.univ-lemans.fr/powbase/
Best,
Armel Le Bail - Universite du Maine, Laboratoire des Fluorures,
CNRS ESA 6010, Av. O. Messiaen, 72085 Le Mans Cedex 9, France
http://www.cristal.org/