I'm looking for structural datas for Tau phases (rhombohedrally deformed
CsCl structure with vacancy ordering) in the AlCuFe and AlCuNi systems. 
I found only one entry in the Crysmet database (ref 130313 NiCu4Al7) and
nothing in ICSD database.


Any hints are welcome.

Patrick.






------------------------------------------------------------------------
------------------------------------------------------------------------
Patrick Weisbecker
LSG2M
Ecole des Mines de Nancy
Parc de saurupt
54042 Nancy
email: [EMAIL PROTECTED]

Reply via email to