This is to indicate that NIST SRMs 640c, silicon powder, and 660a,
lanthanum hexaboride powder, are available from the NIST SRM Program sales
office. These SRMs are certified with respect to lattice parameter at the
part-per-million level. Considerable effort has been expended to tailor
the microstructure of these SRMs to exhibit a minimal level of particle
size and micro-strain induced profile broadening.
Please see:
http://ois.nist.gov/srmcatalog/certificates/view_cert2gif.cfm?certificate=640c
and
http://ois.nist.gov/srmcatalog/certificates/view_cert2gif.cfm?certificate=660a
for views of the certificates which offer a description of the material and
the certification method.
Regards,
Jim
James P. Cline [EMAIL PROTECTED]
Ceramics Division Voice (301) 975 5793
National Institute of Standards and Technology FAX (301) 975 5334
100 Bureau Dr. stop 8523
Gaithersburg, MD 20899-8523 USA
******************************************************************
NIST Standard Reference Materials Program
Phone: 301 975 6776
FAX: 301 948 3730
email: [EMAIL PROTECTED]
Home Page: http://www.nist.gov/srm
> Please see home page for copies of NIST SRM certificates. <
******************************************************************