>From Goodfellows Catalog 2000:
Pd: Thermal Exp. Coeff. (0...100�C) is 11*10E-6 / K
Cheers,
Michael
>
> Hallo everybody
>
> we are desperately seeking the high temperature thermal expansion
> coefficients for PdO (and metallic Pd).
>
> Any information and reference is warmly welcome!!!
>
> G. Artioli
>
>
======================================