Hiya all
We are now the proud owners of a new Bruker D8 system with the twin Goebel
mirror setup (Guinea Pigs R Us!).  This has given me a few headaches with
regard to modelling the instrumental broadening effects (not all of them
solved) but that's another story.  However, for Rietveld work with GSAS I am
at a bit of a loss what value to use for the polarisation factor, as the
diffracted beam mirror is sort of a monochromator but isn't in the
conventional sense.
Any suggestions or ideas would be most welcome.

Best regards
Pam 


Dr Pamela Whitfield  CChem MRSC
Energy Materials Group
ICPET
Building M12
National Research Council
Montreal Road
Ottawa ON
K1A 0R6
Canada

Tel: (613) 991-2435 / (613) 998-8462  
Fax: (613) 991-2384
Email: [EMAIL PROTECTED]

Reply via email to