Hello,

First let me introduce myself. My name is Bill Simon, I just joined the list, after being referred to it by the help staff at ccp14. I'm a graduate student in Materials Engineering at Rutgers University. I'm working on highly textured polycrytalline thin films of Barium Strontium Titanate. I'm looking for a way to properly index each peak in a pole figure. I have used the dot product of the directions, to get the angular seperation, but then there are between 2 and 8 peaks at that angle of Psi. Should I arbitrarily set one peak and work from there?. Thanks in advance.


Bill Simon


Dept. of Ceramic and Materials Engineering
Rutgers University
Piscataway, NJ
08854

ph:     732.445.5567
fax:    732.445.5577