The GUI Powder Instedit function in EXPGUI easily allows you
to create a new instrument parameter file.  It might be
better creating a new file from scratch.

http://www.ncnr.nist.gov/programs/crystallography/software/expgui/expgui.html#INSTEDIT

Lachlan.

-- 
-----------------------
Lachlan M. D. Cranswick
Contact outside working hours /
  Coordonnees en dehors des heures de travail:
E-mail / courriel: [EMAIL PROTECTED]   Home Tel: (613) 584-4226
Mobile/Cell: 613 401 3433   WWW: http://lachlan.bluehaze.com.au/
        P.O. Box 2057, Deep River, Ontario, Canada, K0J 1P0

(please use clear titles in any Email - otherwise messages might
accidentally get put in the SPAM list due to large amount of junk
Email being received. If you don't get an expected reply to any
messages, please try again.)

(Essayez d'utiliser des titres explicites - sans quoi vos messages
pourraient aboutir dans un dossier de rebuts, du fait de la quantite
tres importante de pourriels recue. Si vous n'obtenez pas la reponse
attendue, merci de bien vouloir renvoyer un message.)

Reply via email to