Dear all, I am a newer in magnetic structure determination. I am trying to refining a magnetic structure of double perovskite containing Mn2+ and Mo5+, the nuclear structure is crystallized in P21/n, with Mn (1/2 0 1/2) and W (0 1/2 0). The propagation vector for magnetic cell is (1/2 1/2 0). Can anyone have experience in magnetic refinement write for me the codefile of the magnetic structure, either in P1 or P21/n space group?
Thanks a lot! Qisheng ----- Original Message ----- From: "Frank, Steven" <[EMAIL PROTECTED]> To: <[EMAIL PROTECTED]> Sent: Thursday, July 15, 2004 5:47 PM > Peter, > I received your first message, sorry no generator here. Have you tried > Karl Hofmann at Compass Engineering ([EMAIL PROTECTED])? Good > Luck. > Steve Frank > ANL-W > > -----Original Message----- > From: Peter Zavalij [mailto:[EMAIL PROTECTED] > Sent: Thursday, July 15, 2004 2:11 PM > To: Mailing List, RIETVELD > > Hi everyone, > Sorry for asking again but I am not sure I send this message first time. > I am looking for an old/used generator for Scintag XDS2000 > diffractometer. > New one is too expensive as for old machine. > Any suggestions/contacts are welcome. > Thanks in advance, > > Peter Zavalij > > University Crystallographer > Institute for Materials Research > and Chemistry Department > Binghamton University, SUNY, Vestal Pkwy, East > Binghamton, NY 13902-6000, USA > Tel: (607)777-4298 Fax: (607)777-4623 > E-mail:[EMAIL PROTECTED] > http://materials.binghamton.edu/zavalij > >