I just wanted to remind people interested in magnetic rietveld studies of the programs that perform magnetic symmetry analysis, such as SARAh (ftp.ill.fr/pub/dif/sarah) and BasiReps (included in the FullProf Suite). These programs work out different 'symmetry-allowed' magnetic structures and help in writing the magnetic phases for the refinement (SARAh works with Fullprof and provides a reverse-Monte Carlo refinement engine for GSAS, BasiReps works with Fullprof).
The latest version of SARAh was put on the ILL ftp site this morning (thank you Alan!) and I recommend that users update. I know that Fullprof is updated regularly, so again suggest that users update their installation if it is a little dated...
Best wishes,
Andrew
----------------------------------------------------------------------
Dr. Andrew S. Wills,
Dept. of Chemistry,
Christopher Ingold Laboratories,
University College London,
20 Gordon Street,
London,
WC1H 0AJ,
UK.
Tel: +44 (0) 20 7679 4537
Fax: +44 (0) 20 7679 7463
Email: [EMAIL PROTECTED]
http://www.chem.ucl.ac.uk/people/wills/
On 15 Jul 2004, at 23:04, Qisheng Lin wrote:
Dear all,
I am a newer in magnetic structure determination. I am trying to refining a
magnetic structure of double perovskite containing Mn2+ and Mo5+, the
nuclear structure is crystallized in P21/n, with Mn (1/2 0 1/2) and W (0 1/2
0). The propagation vector for magnetic cell is (1/2 1/2 0). Can anyone have
experience in magnetic refinement write for me the codefile of the magnetic
structure, either in P1 or P21/n space group?
Thanks a lot!
Qisheng