At 08:27 23/07/2004, you wrote:
Could anyone send me the details of the atomic coordinates of LuInO3.

According to ICSD, Lu and In share the perovskite B-site in a tilted oxygen cubic cell IM3- with formula Lu0.5 In0.5 (O H)3 The hydrogen was not located with X-rays, but may occupy the A-site. So just use IM3- perovskite H(Lu,In)O3.

Mullica, D.F.;Sappenfield, E.L.;Gable, D.R. Synthesis, Spectroscopic Studies and Crystal Structure Analysis of 1:1 Lutetium/Indium Trihydroxide28111 (1988) Inorganica Chimica Acta 143, 271-275 XRef
Mullica, D.F.;Sappenfield, E.L.;Gable, D.R.;Tims, T.A. Crystal Structural Analyses of 1:3 (Lu, In) (O H)3 and 1:3 (Yb, In) (O H)3 (1989) Journal of the Less-Common Metals 152, 157-163 XRef


Alan Hewat, ILL Grenoble, FRANCE  <[EMAIL PROTECTED]> fax (33) 4.76.20.76.48
(33) 4.76.20.72.13 (.26 Mme Guillermet) http://www.ill.fr/dif/AlanHewat.htm
___________________________________________________________

Reply via email to