Hello, as the error message tells you, the problem is that there are no reflections at all for one of the patterns. From my experience probable causes for this are 1) wavelength accidently set way too high, 2) lattice parameters accidently set way to low, 3) wrong limits for the observed range given in the pcr-file, 4) dito for the limits or step width given in the data file, 5) indicators, whether a phase contributes to a pattern are all 0 for one pattern or 6) one phase modelled with LeBail mode and no list of reflections is given.
You should check those, I'd bet that one of those is the cause of the problem. Daniel Toebbens On Wed, 25 Aug 2004, Jasminka Popovic wrote: > hello all, > it is me again and again I am in problems. Also I would like to thank you > all for your help with previous problems I had. So the problem regarding > fullprof is: I did my prc file with the help of PCR editor. When I try to > run multi-pattern everything stops in the first cycle with the message: No > reflections found-check your input data. I have the data in free format > 2ThetaI, step, 2ThetaF. I belive that everything with that file is OK since > I can plott it in winplotr. I create a separate folder containing only pcr > and dat file as to make no mistake with those kind of things. So there is > no possibility that I am plotting one file and trying to run other. But > still something is wrong with those input data. Could it be that the data > is fine but I did something wrong in pcr file? > Thank you > Sincerely > > -- > Sudjelujte u Iskon Bonus nagradnom programu i osvajajte nagrade. > Saznajte vi�e na web adresi http://www.iskon.biz/bonus/ > -- ************************************************************************** Daniel M. T�bbens Tel.: +49 30 8062-2793 Hahn-Meitner-Institut / SF2 Fax : +49 30 8062-3172 Glienicker Stra�e 100 D-14109 Berlin, Deutschland http://www.hmi.de/people/toebbens/ **************************************************************************