Hi Andreas

I've been using some thin two sided adhesive tape.

Gilbert TRILLON


-----Message d'origine-----
De : Retief, Johannes (JJ) [mailto:[EMAIL PROTECTED]
Envoy� : jeudi 9 septembre 2004 16:33
� : [EMAIL PROTECTED]
Objet : RE: back loading


Hallo Andreas,

We have been using the cheapest hairspray in town.  Just hold the
aerosol can about 50 cm from the surface and spray gently.
Alternatively, try mixing some instant coffee with the powder.

Regards,

Johannes  



Johannes J. Retief
Sasol Technology (Pty) Ltd
P. O. Box 1
1947 SASOLBURG
South Africa
 
Tel.  : +27 16 960-2940
Fax   : +27 16 960-2826
e-mail: [EMAIL PROTECTED]


-------------------------------------------------------------------------