Can someone please send me the atomic coordinates of Ca and Sr chabazite data.

The IZA (http://www.iza-structure.org/databases/) is a good place to look for info on zeolite structures. If nothing else you can find literature references for CHA structures.


Brian

********************************************************************
Brian H. Toby, Ph.D.                    Leader, Crystallography Team