Dear Stephen,
I have prepared XPD-standard Y2O3 by firing Y2O3 (99.999) from Aldrich
at 1200 �C for 72 hs. (as done in 41-1105 PDF card).
I would also like to ask the other list members if anyone has calibrated
the size-strain broadening of Y2O3 against LaB6, because I have no
access to LaB6 and I've heard that yttria gives broader lines.
Thanks 
Leopoldo

Dr. Leopoldo Suescun
Laboratorio de Cristalograf�a, Estado S�lido y Materiales
(Cryssmat)/Dequifim
Facultad de Qu�mica. CC 1157
Av. Gral. Flores 2124
11800 Montevideo, Uruguay
http://cryssmat.fq.edu.uy/leopoldo/leo.htm

"La emigraci�n es el peor juicio a un r�gimen econ�mico y pol�tico"
                               L�ber Seregni 

-----Mensaje original-----
De: [EMAIL PROTECTED] [mailto:[EMAIL PROTECTED] 
Enviado el: martes, 07 de diciembre de 2004 8:12
Para: [EMAIL PROTECTED]
Asunto: Enquiry of XRD standard materials

Dear Rietvelders,

Does anyone can provide the sources for purchasing XRD standards
materials, such
as CeO2 and Y2O3?

I need few grams of these for calibration of our XRD.

Thank in advance.

regards
stephen