Dear Rietvelders,

in addition to Nita Dragoe's remark: please note that the description of the XRDML file (the "schema") can be found on the website http://www.xrdml.com; it can be used freely by any software developer. With this file format, we tried to get rid of all the issues Nita referred to in his e-mail. We welcome all remarks about this format.

With best regards,
Martijn



Dr. Martijn J. Fransen
Product Manager XRD
PANalytical
Lelyweg 1
7602 EA  Almelo, The Netherlands
Phone ++31 546 534 345
Fax ++ 31 546 534 598
Take a look at our new website! www.panalytical.com






"N. Dragoe" <[EMAIL PROTECTED]>

12/08/2004 01:01 PM
Please respond to
[EMAIL PROTECTED]

To
[EMAIL PROTECTED]
cc
Subject
Re: converting D8focus data





Hi
While it is easier to use directly the raw data file, I preffer  to use
instead ascii files (in ascii files one can easily see the data..).  On of
the problems is that the ascii file may be a little bigger 100K instead of
50k, but this may not be the issue nowadays; in my opinion the real problem
is related to the rather frequent changes of the 'proprietary' format : for
the philips  *.RD data there are several variants, and not all explained
clearly (rd3 to rd5, sd3, sd5..).
One of the solutions might be the use of the recent (public ?) format
xrdml, proposed by Panalytical which is basically an html file. I hear that
this new format is now implemented in Fullprof...
Regards

N

PS  Proprietary means probably that you are not allow to sell software
using this format ???


>What does this mean exactly, proprietary format? That it is secret? I
>am not a very clever programmer, but with the aid of Bruker's own
>manual for their data file conversion utility XCH (to which I
>referred one or two days ago), Appendices A-C, in which the binary
>format is explained in detail, I am able to write a conversion
>utility .raw to .gsas myself in a couple of hours. I did the same
>thing for the conversion of Bruker peak list files (.dif) to Crysfire
>.cdt files. This utility is now distributed with the Crysfire
>distribution.
>And I am not the only one who did this. The LMPG suite of programs
>(Jean Laugier) are all capable to read in Bruker raw files.
>
>Arie

------------------------------
please note the address change :

[EMAIL PROTECTED]
Laboratoire d'Etude des Mat�riaux Hors Equilibre (LEMHE)
UMR 8647 - CNRS
Universit� Paris XI - Bat 410 - 91405 Orsay Cedex - France
Tel: +33.(0)1.69.15.44.48    Fax: +33.(0)1.69.15.48.19
http://www.lemhe.u-psud.fr



Spam detection software, running on the system "lima.ill.fr", has
identified this incoming email as possible spam.  The original message
has been attached to this so you can view it (if it isn't spam) or block
similar future email.  If you have any questions, see
[EMAIL PROTECTED] for details.

Content preview:  This is a multipart message in MIME format.
  --=_alternative 0042E91CC1256F64_Content-Type: text/plain;
  charset="ISO-8859-1" Content-Transfer-Encoding: quoted-printable Dear
  Rietvelders, in addition to Nita Dragoe's remark: please note that the
  description of the XRDML file (the "schema") can be found on the
  website http://www.xrdml.com; it can be used freely by any software
  developer. With this file format, we tried to get rid of all the issues
  Nita referred to in his e-mail. We welcome all remarks about this
  format. [...] 

Content analysis details:   (5.6 points, 5.0 required)

 pts rule name              description
---- ---------------------- --------------------------------------------------
 0.3 NO_REAL_NAME           From: does not include a real name
 0.2 HTML_MESSAGE           BODY: HTML included in message
 5.1 PORN_4                 URI: URL uses words/phrases which indicate porn


Reply via email to