Skip to site navigation (Press enter)
Negative Thermal parameters
Gerard, Garcia S
Mon, 31 Jan 2005 09:06:31 -0800
I'm getting started with GSAS and in all my refinements i get stuck with negative thermal parameters no matter what i do. Is there any tip to get rid of this problem or maybe do i need to learn a little bit more?
Thanks
Previous message
View by thread
View by date
Next message
Re: Negative Thermal parameters
Gerard, Garcia S
Re: Negative Thermal parameters
Norberto Masciocchi
Negative Thermal parameters
Yokochi, Alexandre
Negative Thermal parameters
Whitfield, Pamela
Negative Thermal parameters
Marco Sommariva