> Nanocrystalline phase in films deposited on silica glass substrate:
> After normalization and subtraction of experimentally measured
> substrate pattern, the Rietveld fitting  (GSAS) of the
> Nanocrystalline phase becomes worst than the case of mathematically
> modelled background.
>
> Which is the best way to handle this problem? experimental (and how?)
> or mathematical modelling?

Try DDM metod - it is independent of the background.
http://krsk.info/icct/en/cont/persons/sol/ddm.html

Regards,
Leonid



                