Hi Kosta, Although I haven't used GSAS, I have encountered the problem of low peak intensities using Rietveld method. In the case of my samples it was preferred orientation of the crystals (that is, rather experimental error during sample preparation than software problem) that caused low calculated peak intensities, although the observed peaks on the pattern seemed to correspond in higher intensities. By the way, nice to find another Greek in this list! Regards Sarra
-----Original Message----- From: Papangelis Konstantinos [mailto:[EMAIL PROTECTED] Sent: Thursday, March 03, 2005 9:46 AM To: [email protected] Dear all I am trying to do Le Bail fitting (GSAS) on sychrotron XRD data (capillary). Although the peak positions fit nice the calculated intensities are extremely low. The chisquare increases dramatically after a few iterations. Note that the background is not so smooth. I would appreciate if someone could advise me. Best regards Kostas