>I am trying to do Le Bail fitting (GSAS) on sychrotron XRD data (capillary).
>Although the peak positions fit nice the calculated intensities are
>extremely low.

Not sure with GSAS, but try to decrease the fixed scale factor,
and the extracted intensities should increase ?

Armel



Reply via email to