Mr. Karagianni,

 

There was a round robin study conducted by the International Union of Crystallography and also by ASTM and NIST in the U.S.. The results of the IUCr round robin are published in Madsen, C., Scarlett, N.V.Y., Cranswick, L.M.D. & Lwin, T.

2001. Outcomes of the International Union of

Crystallography Commission on Powder Diffraction round

robin on quantitative phase analysis: samples 1a to 1h. J.

Appl. Cryst. 34: 409-426.

 

I am sending you a link with a lot of relevant links and publications. I am not aware whether there is a current study, but if you need pertinent results for your work, you will find a lot in there.

 

http://www.ccp14.ac.uk/solution/rietveld_and_esds/

 

I hope this helps,

 

Maria Chrysochoou

W.M. Keck Geoenvironmental Laboratory

Stevens Institute of Technology

Tel.: +1 201 216 8773

Fax: +1 201 216 8212

E-mail: [EMAIL PROTECTED]

 

-----Original Message-----
From: [EMAIL PROTECTED] [mailto:[EMAIL PROTECTED]
Sent: Wednesday, June 08, 2005 4:18 AM
To: Rietveld Mailing List
Subject: Rietveld Round Robin Test

 


Fellow rietvelders,

Is there any round robin test (official or not) for Rietveld? I am particularly interested in cement and clinker phase refinement.

Thank you.


John Karagiannis
Hellenic Cement Research Center Ltd. \ Microstructure Dept
K. Pateli 15
ATHENS ATTICA 141 23
GREECE
Fax:   0030-210-2842140
Tel:   0030-210-2818453


=======================================================
The Heracles G.C.C. Group of Companies wishes to make it known
that:
This email and any attachments are confidential and solely for the use of the intended recipient. They may contain material protected by professional privilege. If you are not the intended recipient or the person responsible for delivering to the intended recipient, you are not
authorized to and must not disclose, copy, distribute or retain this
email or its attachments. Although this email and its attachments are believed to be free of any virus or other defect, it is the responsibility
of the recipient to ensure that they are virus free and no responsibility is accepted by the sender for any loss or damage arising from receipt or use thereof. Anything contained in this message that does no relate to the official business of a Group's Company shall be understood as neither sent not endorsed by the Group.Furthermore , it is noted that each Company of the Group undertakes commitments towards third parties only in the manner prescribed in its Statutes.

Reply via email to