There were two papers resulting from a round robin on quantitative phase analysis sponsored by the IUCr Commission on Powder Diffraction. They are:-
 
(1)    I.C. Madsen, N.V.Y. Scarlet, L.M.D. Cranswick, T. Lwin, J. Appl Cryst. (2001) 34, 409-426

(2)    N.V.Y. Scarlet, I.C. Madsen, L.M.D. Cranswick, T. Lwin, E. Groleau, G. Stephenson, M. Aylmore, N. Agron-Olshina, J. Appl Cryst. (2002) 35, 383-400 

The second paper deals with the more complex phase systems. If you do not have access to J.Appl.Cryst. let me know and I will send reprints.

During the design of the round robin we contemplated using cement materials but were concerned about the long-term stability of clinker

 
 
Cheers
 
o----------------------oo0oo---------------------------o
     Ian Madsen
     CSIRO Minerals
     Box 312
     Clayton South 3169
     Victoria
     AUSTRALIA
     Phone +61 3 9545 8785 direct
                 +61 3 9545 8500 switch
                 +61 (0) 417 554 935 mobile
     FAX    +61 3 9562 8919
     Email [EMAIL PROTECTED]
o----------------------oo0oo---------------------------o
-----Original Message-----
From: [EMAIL PROTECTED] [mailto:[EMAIL PROTECTED]
Sent: Wednesday, 8 June 2005 7:18 PM
To: Rietveld Mailing List
Subject: Rietveld Round Robin Test


Fellow rietvelders,

Is there any round robin test (official or not) for Rietveld? I am particularly interested in cement and clinker phase refinement.

Thank you.


John Karagiannis
Hellenic Cement Research Center Ltd. \ Microstructure Dept
K. Pateli 15
ATHENS ATTICA 141 23
GREECE
Fax:   0030-210-2842140
Tel:   0030-210-2818453


=======================================================
The Heracles G.C.C. Group of Companies wishes to make it known
that:
This email and any attachments are confidential and solely for the use of the intended recipient. They may contain material protected by professional privilege. If you are not the intended recipient or the person responsible for delivering to the intended recipient, you are not
authorized to and must not disclose, copy, distribute or retain this
email or its attachments. Although this email and its attachments are believed to be free of any virus or other defect, it is the responsibility
of the recipient to ensure that they are virus free and no responsibility is accepted by the sender for any loss or damage arising from receipt or use thereof. Anything contained in this message that does no relate to the official business of a Group's Company shall be understood as neither sent not endorsed by the Group.Furthermore , it is noted that each Company of the Group undertakes commitments towards third parties only in the manner prescribed in its Statutes.

Reply via email to