particularly if texture occurs for one or many phases !

daniel


>
> Dear Maria,
>
> I agree with Dr. Retief, I would never refine structure details like
> atomic
> coordinates or temperature factor (displacement factors) for QPA!
> Regards
> Francois Girod
>
>
>
>
>                               "Retief, Johannes
>                               \(JJ\)"                      Pour
> :<[email protected]>
>                               <[EMAIL PROTECTED]        cc :
>                               l.com>                       Objet:RE:
> Question on temperature factors
>
>                               01.07.2005 08:50 ZE2
>                               Veuillez répondre à
>                               rietveld_l
>
>
>
>
>
> Hallo Maria,
>
> Temperature factors are strongly correlated with surface roughness.
> Refining them using X-rays easily lead to rediculously large positive
> values or even negative values.  My advice would be to fix them at the
> theoretical values, especially for the QPA of a complicated system.
>
> Regards,
>
> Johannes Retief
>
>
>
>       -----Original Message-----
>       From: Maria Chrysochoou [mailto:[EMAIL PROTECTED]
>       Sent: 30 June 2005 21:55
>       To: [email protected]
>       Subject: Question on temperature factors
>
>       Hi all,
>
>       I have a question on temperature factors in Rietveld refinement.
>       I am on working on a complicated system with over 12 phases on
>       average (it is cement-like in chemistry and mineralogy). I tend not
>       to refine temperature factors in order to reduce the number of
>       refinable parameters to a realistic number.
>       Do you think that the temperature factors make a big difference in
>       quantitative analysis? Could you give me a range of reasonable
> values
>       for an ambient temperature cement?
>
>       Thank you,
>
>       Maria Chrysochoou
>       W.M. Keck Geoenvironmental Laboratory
>       Stevens Institute of Technology
>       Tel.: +1 201 216 8773
>       Fax: +1 201 216 8212
>       E-mail: [EMAIL PROTECTED]
>
>
>
>
>
>
>
>
>
> NOTICE: Please note that this eMail, and the contents thereof, is subject
> to the standard Sasol eMail legal notice which may be found at:
> http://www.sasol.com/legalnotices
>
>
> If you cannot access the legal notice through the URL attached and you
> wish
> to receive a copy thereof please send an eMail to [EMAIL PROTECTED]
>
>
>
>
>
>
>
>
>
>


-- 
Daniel Chateigner
Professeur
CRISMAT-ENSICAEN
Bd. M. Juin
14050 Caen, France
http://www.ecole.ensicaen.fr/~chateign/danielc/

Reply via email to