While on the topic of mail-in facilities and readily available neutrons for the powder diffraction community (North American based in this case).
The C2 neutron powder diffractometer at Chalk River, Ontario, Canada has a rolling proposal system where users can submit beamtime proposals at any time. After the proposal has been approved, users often take the option of using a mail-in system. C2 is an 80 degree, 800 wire PSD system. Web information: English: http://neutron.nrc-cnrc.gc.ca/c2gen.html Francais: http://neutron.nrc-cnrc.gc.ca/fch/c2gen.html Proposal form is available on the web (and again, can be submitted at any time as part of rolling review process): http://neutron.nrc-cnrc.gc.ca/propfrm.html http://neutron.nrc-cnrc.gc.ca/fch/propfrm.html ---------- If requiring data for solving structures by Fox (or similar structure solution programs): Sample run at ~2.37 A (single bank 5 to 85 degrees 2-theta) For refining: Sample run at ~1.33 A (two bank merged data, 5 to 115 degrees 2-theta) If unit cell "accuracy" (rather than "precision") is required at a range of temperatures (including RT): Extra run at ~1.33 A with high purity platinum foil standard, single 80 degree bank of data. ------------ Lachlan -- ----------------------- Lachlan M. D. Cranswick Contact outside working hours / Coordonnees en dehors des heures de travail: E-mail / courriel: [EMAIL PROTECTED] Home Tel: (613) 584-4226 Mobile/Cell: 613 401 3433 WWW: http://lachlan.bluehaze.com.au/ P.O. Box 2057, Deep River, Ontario, Canada, K0J 1P0 (please use clear titles in any Email - otherwise messages might accidentally get put in the SPAM list due to large amount of junk Email being received. If you don't get an expected reply to any messages, please try again.) (Essayez d'utiliser des titres explicites - sans quoi vos messages pourraient aboutir dans un dossier de rebuts, du fait de la quantite tres importante de pourriels recue. Si vous n'obtenez pas la reponse attendue, merci de bien vouloir renvoyer un message.)