I´m refining a sample which contains a hydroxycarbofluorapatite (solid solution). I´m refining it using CIF files from the ICSD, but it´s not working so well, because they don´t have the file for the hydroxycarbofluorapatite. So I´m using in the TOPAS the following files: fluorapatite, carbofluorapatite, hydroxyfluorapatite and hydroxyapatite. When using them the rwp is about 16 but when using only the hydroxyapatite the rwp is 30. I´d would like to know if any of you have very good quality STR files of hydroxyapatite, fluorapatite and carboapatite, or only one file of hydroxycarbofluorapatite?!