Dear all,

We have had some problems with our Ni/C 60mm length Gobel (Goebel)
mirrors. 
I believe "2nd Generation" purchased 2003. 

We now realise that over a period of time deposits have built up in the
mirror giving up to 60% reduction in intensity and additional low
intensity "peaks".

I was wondering if this is an issue known to the community. Bruker can
refurbish our original mirrors. Anyone have knowledge of how efficient
this process is?

If you have had similar problems and have fixed them please get in
touch.

Regards

Tim Hyde

Dr Tim Hyde
Principal Scientist
Johnson Matthey Technology Centre
Blounts Court
Sonning Common
Reading RG4 9NH

Tel: +44 (0) 118 924 2152
Fax: +44 (0) 118 924 2254
email [EMAIL PROTECTED]


If the reader of this email is not the intended recipient(s), please be advised 
that any dissemination, distribution or copying of this information is strictly 
prohibited. Johnson Matthey PLC has its main place of business at 40-42 Hatton 
Garden, London (020 7269 8400).

Johnson Matthey Public Limited Company
Registered Office: 40-42 Hatton Garden, London EC1N 8EE
Registered in England No 33774

Whilst Johnson Matthey aims to keep its network free from viruses you should 
note that we are unable to scan certain emails, particularly if any part is 
encrypted or password-protected, and accordingly you are strongly advised to 
check this email and any attachments for viruses. The company shall NOT ACCEPT 
any liability with regard to computer viruses transferred by way of email.

Please note that your communication may be monitored in accordance with Johnson 
Matthey internal policy documentation.

Reply via email to