MessageDear Judy

Yes, it is a symbol for the structure of NaZn13, the working material of my 
collaborator. Neverteless, the Shoenfiles symbol D23 seems to be equivalent to 
Fm3-c. Thanks everyone for the help.

Best wishes
Jana



  ----- Original Message ----- 
  From: Judith Stalick 
  To: [email protected] 
  Sent: Monday, January 28, 2008 4:17 PM
  Subject: Re: RE:


  Jana,

  It sounds like the Strukturbericht designation for the NaZn13 structure type.

  Judy Stalick

    ----- Original Message ----- 
    From: Von Dreele, Robert B. 
    To: [email protected] 
    Sent: Monday, January 28, 2008 10:09 AM
    Subject: RE:


    Hi,
    Not sure - need to know the context. It may be a mistyped Shoenflies symbol 
for either space group P 21 21 2 (orthorhombic) or P321 (trigonal).
    Bob Von Dreele


    R.B. Von Dreele

    IPNS Division

    Argonne National Laboratory

    Argonne, IL 60439-4814

     

      -----Original Message-----
      From: Jana Bezjak [mailto:[EMAIL PROTECTED] 
      Sent: Monday, January 28, 2008 7:43 AM
      To: [email protected]
      Subject: 


      Dear

      I would like to ask you for the explanation of the crystallographic 
notation D23

      Thank you

      Jana
  __________ NOD32 2799 (20080116) Information __________

  This message was checked by NOD32 antivirus system.
  part000.txt - error - unknown compression method 

  http://www.eset.com

Reply via email to