MessageJana,

It sounds like the Strukturbericht designation for the NaZn13 structure type.

Judy Stalick

  ----- Original Message ----- 
  From: Von Dreele, Robert B. 
  To: [email protected] 
  Sent: Monday, January 28, 2008 10:09 AM
  Subject: RE:


  Hi,
  Not sure - need to know the context. It may be a mistyped Shoenflies symbol 
for either space group P 21 21 2 (orthorhombic) or P321 (trigonal).
  Bob Von Dreele


  R.B. Von Dreele

  IPNS Division

  Argonne National Laboratory

  Argonne, IL 60439-4814

   

    -----Original Message-----
    From: Jana Bezjak [mailto:[EMAIL PROTECTED] 
    Sent: Monday, January 28, 2008 7:43 AM
    To: [email protected]
    Subject: 


    Dear

    I would like to ask you for the explanation of the crystallographic 
notation D23

    Thank you

    Jana

    Jana Bezjak
    Jozef Stefan Institute
    Jamova 39
    SI-1000 Ljubljana, Slovenia
    Advanced Materials Department
    +386 (0)1 477-35-47

Reply via email to