>Leonid, I suggest you to try K4P2O7 - synchrotron data...

If you send me the data I may try.

OK.

K4P2O7 at room temperature is a good example for your horror museum of bad things done in the SDPD world and which could have been so much better if DDM was used.

This case belongs to the acentric class of problems. Acentricity leads to a 2 times more unfavourable (atomic coordinates)/data ratio than for centric compounds. This is also the case for beta-Ba3AlF9 for which I can send the original 1993 data, if you wish, and you may see if Al-F distances are convincing without restraints using DDM (I obtained crazy Al-F distances in the 1.65-1.97 A range, instead of 1.81+-0.04 A for usually regular AlF6 octahedra).

BTW, try to solve the structure before the Rietveld fif.

Best,

Armel

++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++