Tubetails are simply the result of emission of the target radiation from outside the wanted line focus, some mm around. Depending on tube quality, age and operating power, one can have varying shapes when projected on the 2theta scale. Examples:
http://www.bgmn.de/tubetails.html
As you can see, the shape are not hats as assumed in Topas but may have discrete maxima at both sides, may by assymetric. Especially for sharp peaks, the correction strongly improves the result of profile fitting:

Bergmann, J., Kleeberg, R., Haase, A., Breidenstein, B. (2000) Advanced fundamental parameter model for improved profile analysis. Mat. Sci. Forum Vols. 347-349(2)303-308.


In general, the tubetails more strongly influence the peak shape for instruments with smaller goniometer radius and when the equatorial divergence slit is placed closer to the sample. In general. Alan's statement that the width/shape of the tubetails is 2Th independent is correct, as it is simply a projection on the measuring circle. But, as a part of the tubetails diffracted intensity is generated outside the projection of the wanted focus via the divergence slit on the sample, tubetails may be cut by a limited size of the sample. Such cutting of the tubetails effect may happen at low angles for fixed slit systems and at higher angles when using automatic slit systems. In consequence, the intensity and shape of the tails effect can become dependent on 2Theta, in a complicated way. In BGMN/GEOMET we try to convolute an experimentally measured focus profile into the geometrical contribution of the MonteCarlo simulation. As this procedure is done at discrete angular steps and the resulting geometrical profiles are interpolated later, we hope to have introduced correctly such secondary effects.

Reinhard

Am 17/09/2013 03:53, schrieb Alan Coelho:
Matt

I am not sure I understand how you would account for the additional
wavelengths in the beam.
Tube tails is spectrally independent and its aberration shape is 2Th
independent. Its realized in TOPAS by a convolution called stacked_hats
which, as its name suggests, convolutes a series of stacked impulse
functions. An intense narrow hat represents the beam and wider hats the
penetration of the electrons in the tube.

Cheers
Alan

-----Original Message-----
From: Matt Beekman [mailto:[email protected]]
Sent: Tuesday, 17 September 2013 2:08 AM
To: Peter Y. Zavalij; Alan Coelho; [email protected];
[email protected]
Subject: RE: Instrumental resolution function

Alan, Peter,

Would you mind briefly elaborating on the procedure used to "fit tube
tails?" I personally have only used GSAS for Rietveld refinement, and other
than adding another phase(s) with slightly different lattice parameter(s) I
am not sure I understand how you would account for the additional
wavelengths in the beam.

Many thanks in advance!

Matt

--
Matt Beekman, Ph.D.
Assistant Professor of Physics
Department of Natural Sciences
Oregon Institute of Technology
3201 Campus Drive
Klamath Falls, OR 97601
Tel: 541-885-1940
Fax: 541-885-1849
Email: [email protected]
Web:
http://www.oit.edu/faculty-staff/home-pages/natural-science/matt-beekman



-----Original Message-----
From: [email protected] [mailto:[email protected]] On Behalf
Of Peter Y. Zavalij
Sent: Monday, September 16, 2013 6:11 AM
To: Alan Coelho; [email protected]; [email protected]
Subject: RE: Instrumental resolution function

I do exactly the same - fit tube tails using LaB6 standard and use the
parameters (usually w/o fitting) in all other refinements. Although tube
tails fitting helps a lot it's not perfect.
Peter Zavalij

-----Original Message-----
From: Alan Coelho [mailto:[email protected]]
Sent: Sunday, September 15, 2013 10:05 PM
To: Peter Y. Zavalij; [email protected]; [email protected]
Subject: RE: Instrumental resolution function

Hi Peter, Mario

I happen to have a Ni filter, Cu, LaB6 pattern  that has a very similar look
to the one sent by Mario. Probably best to look at the 21.35 degrees 2Th
peak. The Ni filter cut-off occurs at 20.6 degrees 2Th, the satellite group
is hard to see due to the low angle and hence compression of the emission
profile. What made sense in the pattern was to fit Tube tails. Across the
whole patter the Rwp was reduced by 2.1% where Tube tails was considered and
the fit at the shoulders was good.

Cheers
Alan


-----Original Message-----
From: [email protected] [mailto:[email protected]] On Behalf
Of Peter Y. Zavalij
Sent: Monday, 16 September 2013 10:55 AM
To: [email protected]; [email protected]
Subject: RE: Instrumental resolution function

Hi Mario,
The shoulder you observe is what's left from "white" after it is cut off by
beta-filer. You could check the absorption edge of Ni and it is right at the
shoulder you observe.
Peter

__________________________________
Peter Zavalij
X-ray Crystallographic Center
University of Maryland
College Park, MD 20742
Phone/Fax: (301)405-1861
http:/www.chem.umd.edu/crystallography



-----Original Message-----
From: [email protected] [mailto:[email protected]] On Behalf
Of [email protected]
Sent: Sunday, September 15, 2013 6:08 PM
To: [email protected]
Subject: Instrumental resolution function

Dear All,

I am calculating the corresponding instrumental resolution function of our
Bruker diffractometer which is operating in Bragg-Brentano geometry with Cu
radiation, using a nickel filter and LynxEye detector.

The calculation is carried out by the Rietveld analysis of the LaB6 (660b)
NIST-standard. We observed the Kbeta peaks, but also some shoulders in the
left part of the peaks. We have some ideas about this but taking into
account that I'm not an actual expert, your comments will be very important
to me.

In the attached file, I send an image to make a better illustration of my
doubts.

Thanks in advance for your help.
Best Regards,

Mario A. MacĂ­as
Universidad Industrial de Santander
Bucaramanga-Colombia.




--
TU Bergakademie Freiberg
Dr. R. Kleeberg
Mineralogisches Labor
Brennhausgasse 14
D-09596 Freiberg

Tel.    ++49 (0) 3731-39-3244
Fax. ++49 (0) 3731-39-3129

++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <[email protected]>
Send commands to <[email protected]> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/[email protected]/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++

Reply via email to