Dear Rietvelders,

 

I decided to completely embarrass myself and ask you a simple phase
identification question. I’ve had some trouble in trying to figure out
what’s going on with one measurement done in our lab. The sample is a ~30nm
film heat treated in air at 500C, composition is Ce:Sn in close to 1:1 ratio
plus oxygen in addition to those. I can’t tell if there’s any very light
elements as we only have EDX data at the moment, and the actual amount of O
is still unclear due to 3-4nm of native SiO2 under the sample and I don’t
have any XPS/RBS/SIMS profile data yet. I can’t find anything from our
databases that would fit even remotely close to the measured data. (we have
ages old PDF2 but I’ve imported every CeOx, SnOx and CexSnyOz structure I
could find from latest ICSD). Indexing is a bit frustrating as well since I
can’t be sure if it’s a single phase, and I don’t have too much experience
with unknowns anyway. 

 

The measurement was done in grazing incidence mode with 1deg incident angle
(it seems that there was some 0.014deg of 2theta shift back then).  I’ve
done rocking curve measurements from the first six reflections, based on
that it doesn’t seem to be textured so there shouldn’t be reflections
missing due to that (particle statistics is obviously a different matter…).
When measuring with different incident angles (from 0.25 to 3.75 2th) the
diffractograms don’t seem to change, so there’s probably no separate layers
but one homogeneous matter. The data is found here for those interesting in
trying: http://www.helsinki.fi/~mwheikki/temp/  And before you ask, there’s
no reflections below the one at 23.5 2th. And it’s a Cu tube.

 

I really appreciate any effort and time any of you might spend with the
data. I’m currently trying to find something from the literature but no
success so far. Hopefully you can make me feel stupid and find out the easy
solution before I do J

 

Have a nice weekend!

 

BR,

Mikko

 

---

Mikko Heikkilä, M.Sc., Laboratory engineer

Laboratory of Inorganic Chemistry

Department of Chemistry

P.O. Box 55 (A.I. Virtasen aukio 1)

FI-00014 University of Helsinki

 

phone:   +358919150216

mobile:  +358504160572

email: [email protected]

 

++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <[email protected]>
Send commands to <[email protected]> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/[email protected]/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++

Reply via email to