Dear Natale,

do you think about a Gandolfi like setup? Or can the fragments be crushed?

best

Miguel


---
michele gregorkiewitz
Dip Scienze Fisiche, della Terra e dell'Ambiente
Università di Siena
via Laterina 8, I-53100 Siena
[email protected], +39'0577'233810


Il 2015-07-29 11:33 Natale Perchiazzi ha scritto:
Dear All,
I would need to get good quality powder pattern, suitable for Rietveld
analysys, working on mineral microcrystalline fragments with
dimensions around 0.1-0.2 mm. From your experience, which could be an
European synchrotron beamline with a suitable experimental setup to
get these data?
best regards Natale Perchiazzi
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <[email protected]>
Send commands to <[email protected]> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/[email protected]/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++

Reply via email to