Dear Natale,

Why you are not collecting single crystal data with such beautiful crystals?

For powders the best beamline is that one which will be the first to give you 
the beamtime☺


Radovan Cerny
Laboratoire de Cristallographie, DQMP
Université de Genève
24, quai Ernest-Ansermet
CH-1211 Geneva 4, Switzerland
Phone  : [+[41] 22] 37 964 50, FAX : [+[41] 22] 37 961 08
mailto : [email protected]
URL    : http://www.unige.ch/sciences/crystal/cerny/rcerny.htm

De : [email protected] [mailto:[email protected]] De la part de 
Natale Perchiazzi
Envoyé : mercredi 29 juillet 2015 11:34
À : Lista Rietveld
Objet : synchrotron beamline info

Dear All,
I would need to get good quality powder pattern, suitable for Rietveld 
analysys, working on mineral microcrystalline fragments with dimensions around 
0.1-0.2 mm. From your experience, which could be an European synchrotron 
beamline with a suitable experimental setup to get  these data?
best regards        Natale Perchiazzi
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <[email protected]>
Send commands to <[email protected]> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/[email protected]/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++

Reply via email to