About ten years ago, I was working on a D4 with lynx eye, And had to put an air scatter blocker 1 or 2 mm above the powder sample with fixture on the stage. In the beginning, I had to put simple geometry into the bgmn configuration sav-file until Dr Bergmann put a parameter airscatter=#.

Now I came back to the same business with a D8 with lynx eye; is there anybody here willing to share the experience of handling it in TOPAZ?