Hi Matthew,

what you mentioned earlier is not completely correct:

An anti-air scatter (or beam knife) does not only reduce background (mainly at low angles), but also cuts intensity at higher 2theta values, if not installed correctly. It does not result in a sample displacement error, it just cuts intensity as it cuts off the beam like you mentioned. This is also an relatively easy issue to modell, I even managed to put it into an excel-file to calculate the max. 2theta angle that can be measured at a certain knife height and detector length. BGMN "handles" this properly as well. Nowadays, there are even knifes available that move vertically, depending on the actual 2theta value.

In general, a beam knife would not be necessary if the optics worked properly, i.e. the optical path is not disturbed or diffracted or fluorescence would not be generated somewhere in the beam path. Basing on our experience, the main source of these unwanted X-rays are within or close to the tube itself, making it hard to suppress it effectively. All these things result in some strange background phenomena at low angles (bumps/edges...). We discussed these issues with Reinhard Kleeberg and others for a while. It seems to be a serious problem in modern devices, as we experienced this on our own PANalytical and other (Bruker) devices from colleagues.

Regards,

Robert



, 30 Jul 2015 11:53:15 +0800 schrieb Matthew Rowles <[email protected]>:
Hi Jilin

You could probably add a note to your input file.

Not everything you use in your hardware can be either properly modelled, or
influence the pattern significantly. Do you need to model the anti-scatter
slits? They help reduce background.

One thing that could happen is that if the knife is set up incorrectly, it
will cut off the beam, shifting the centroid of diffraction. That may mimic
a sample displacement type error.

Re your comment about double-digit results. Are you talking about the quant
results given in the GUI? The actual answer is going to be a lot less
precise than that.


Matthew









On 30 July 2015 at 09:19, ji zhang <[email protected]> wrote:



Matthew

I was thinking shouldn't we be able to input some parameters to reflect
this hardware configuration in the program?

I forgot that I had asked the same question in2007 in this list. Nobody
seemed to care enough except Dr Bergmann. Then I went to do log analysis,
and this thing is completely forgotten.

Currently we have topaz where I can't find a way to circumvent this yet or
to handle this as I called it. I am thinking we may need a copy of bgmn.
Certainly both give double digit results (albeit not the same) and both
look accurate.



Sent from Yahoo Mail for iPhone <https://yho.com/footer0>

On Jul 29, 2015, 5:56:41 PM, Matthew Rowles wrote:

Hi

What do you mean by "handle it"?

If the knife edge is correctly set up, the only thing that should change
is the background.

Matthew Rowles
On 30 Jul 2015 3:04 am, "ji zhang" <[email protected]> wrote:


About ten years ago, I was working on a D4 with lynx eye, had to put an
air scatter blocker 1 or 2 mm above the powder sample. In the beginning, I
had to put simple geometry into the bgmn configuration sav-file until Dr
Bergmann put a parameter airscatter=#.

Now I came back to the business with a D8 with lynx eye; is there anybody
here willing to share the experience of handling it in TOPAZ?

thanks

Jilin zhang

Sent from Yahoo Mail for iPhone <https://yho.com/footer0>

++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list
Send commands to <[email protected]> eg: HELP as the subject with no body
text
The Rietveld_L list archive is on
http://www.mail-archive.com/[email protected]/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++




---
Dr. rer. nat. Robert Möckel
Diplom-Mineraloge
Helmholtz-Institut Freiberg für Ressourcentechnologie
Tel.:  +49 (0) 3731 39 2079
Helmholtz-Zentrum Dresden-Rossendorf
Halsbrücker Str. 34 | 09599 Freiberg
http://www.hzdr.de/hif | [email protected]
Vorstand: Prof. Dr. Dr. h. c. Roland Sauerbrey | Prof. Dr. Dr. h. c. Peter Joehnk | VR 1693 beim Amtsgericht Dresden
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <[email protected]>
Send commands to <[email protected]> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/[email protected]/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++

Reply via email to