Hi all
I have done it in the past by changing the "refine flag" in the
intensity list of the Pawley refinement with a fake scale factor (one
per dataset - minus the "0th one") multiplying the intensity values of
each reflection.
Just use TOPAS in launch mode.
Norberto
Dear all,
I would like to obtain integrated intensities from several (up to 5)
powder patterns that were measured at different temperatures.
My idea is to make fit by Pawley (or Le Bail?) method of all datasets
at the same time and keep integrated intensities of individual hkls
the same for all datasets.
Do you know about some software, that can restrain or even fix
integrated intensities between refined datasets?
Thank you in advance,
Jan
/Ing. Jan Rohlicek, Ph.D./
/Institute of Physics CAS//
Cukrovarnicka 10/112
162 00 Prague 6/
/Tel: (+420) 220 318 484/
/Email: [email protected]///
<http://www.avg.com/email-signature?utm_medium=email&utm_source=link&utm_campaign=sig-email&utm_content=emailclient>
Mail priva di virus. www.avg.com
<http://www.avg.com/email-signature?utm_medium=email&utm_source=link&utm_campaign=sig-email&utm_content=emailclient>
<#DAB4FAD8-2DD7-40BB-A1B8-4E2AA1F9FDF2>
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <[email protected]>
Send commands to <[email protected]> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/[email protected]/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
--
Norberto Masciocchi
Professor of Chemistry
Department of Science and High Technology & To.Sca.Lab.
University of Insubria
Via Valleggio, 11
22100 Como - Italy
E-mail: [email protected]
Tel: +39-031-2386613
Skype: norberto.masciocchi
Website: toscalab.uninsubria.it
Publish in: Chem2 Journal (www.chem2.org)!
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <[email protected]>
Send commands to <[email protected]> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/[email protected]/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++