A second vote for Topas. You can have multiple hkl phases and do a Pawley
refinement. The intensities can be given the same keyword, which forces
them to have the same value. You then refine a scale factor on patterns
2-5, with the 1st one fixed at 1.

Matthew

On 6 June 2018 at 17:02, Norberto Masciocchi <
[email protected]> wrote:

> Hi all
> I have done it in the past by changing the "refine flag" in the intensity
> list of the Pawley refinement with a fake scale factor (one per dataset -
> minus the "0th one")  multiplying the intensity values of each reflection.
> Just use TOPAS in launch mode.
> Norberto
>
> Dear all,
>
>
>
> I would like to obtain integrated intensities from several (up to 5)
> powder patterns that were measured at different temperatures.
>
> My idea is to make fit by Pawley (or Le Bail?) method of all datasets at
> the same time and keep integrated intensities of individual hkls the same
> for all datasets.
>
>
>
> Do you know about some software, that can restrain or even fix integrated
> intensities between refined datasets?
>
>
>
> Thank you in advance,
>
> Jan
>
>
>
> *Ing. Jan Rohlicek, Ph.D.*
>
> *Institute of Physics CAS*
>
> * Cukrovarnicka 10/112 162 00 Prague 6*
>
> *Tel: (+420) 220 318 484*
>
> *Email: [email protected] <[email protected]>*
>
>
>
>
> <http://www.avg.com/email-signature?utm_medium=email&utm_source=link&utm_campaign=sig-email&utm_content=emailclient>
>  Mail
> priva di virus. www.avg.com
> <http://www.avg.com/email-signature?utm_medium=email&utm_source=link&utm_campaign=sig-email&utm_content=emailclient>
> <#m_5331402660391734722_DAB4FAD8-2DD7-40BB-A1B8-4E2AA1F9FDF2>
>
> ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
> Please do NOT attach files to the whole list <[email protected]> 
> <[email protected]>
> Send commands to <[email protected]> <[email protected]> eg: HELP as the subject 
> with no body text
> The Rietveld_L list archive is on 
> http://www.mail-archive.com/[email protected]/
> ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
>
>
>
> --
> Norberto Masciocchi
> Professor of Chemistry
> Department of Science and High Technology & To.Sca.Lab.
> University of Insubria
> Via Valleggio, 11
> 22100 Como - Italy
> E-mail: [email protected]
> Tel: +39-031-2386613
> Skype: norberto.masciocchi
> Website: toscalab.uninsubria.it
> Publish in: Chem2 Journal (www.chem2.org)!
>
>
>
> ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
> Please do NOT attach files to the whole list <[email protected]
> >
> Send commands to <[email protected]> eg: HELP as the subject with no body
> text
> The Rietveld_L list archive is on http://www.mail-archive.com/
> [email protected]/
> ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
>
>
>
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <[email protected]>
Send commands to <[email protected]> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/[email protected]/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++

Reply via email to