Hi Claire

If you just model the phase with generic peaks, and no scale factor, it
will be excluded from the Hill & Howard quantification algorithm. You're
now in relative weight fraction world, and everything is scaled to 100%.
You could also try DDM (Toraya 2016 and others) if you're keen, but
depending on your aversion to patents, you might not want to.

Matthew

On Wed, 1 Nov 2023 at 00:19, Claire Emily Boronski <
[email protected]> wrote:

> Hi All,
>
>
>
> I am trying to fit a large unknown amorphous phase. It is not being
> properly fit by my background and being fit by broadening out the peaks of
> other small phases present that should be crystalline. I did XRD-CT on a
> lead pipe scale material and so I cannot spike the sample with a known
> weight percentage of material with a similar absorption coefficient. Is
> there any way that I can fit this unknown phase as just a general unknown
> amorphous material and exclude it from the weight percent calculation?
>
>
>
> Thanks,
>
> Claire
>
>
> ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
> Please do NOT attach files to the whole list <[email protected]
> >
> Send commands to <[email protected]> eg: HELP as the subject with no body
> text
> The Rietveld_L list archive is on
> http://www.mail-archive.com/[email protected]/
> ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
>
>
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
Please do NOT attach files to the whole list <[email protected]>
Send commands to <[email protected]> eg: HELP as the subject with no body text
The Rietveld_L list archive is on http://www.mail-archive.com/[email protected]/
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++

Reply via email to